Skip to main page content
U.S. flag

An official website of the United States government

Dot gov

The .gov means it’s official.
Federal government websites often end in .gov or .mil. Before sharing sensitive information, make sure you’re on a federal government site.

Https

The site is secure.
The https:// ensures that you are connecting to the official website and that any information you provide is encrypted and transmitted securely.

Access keys NCBI Homepage MyNCBI Homepage Main Content Main Navigation
. 1999 Jun;16(6):847-53.
doi: 10.1023/a:1018822002353.

pH and osmotic pressure inside biodegradable microspheres during erosion

Affiliations

pH and osmotic pressure inside biodegradable microspheres during erosion

A Brunner et al. Pharm Res. 1999 Jun.

Abstract

Purpose: To measure changes in pH as well as osmotic pressure in aqueous pores and cavities inside biodegradable microspheres made from polymers such as poly(D,L-lactic acid) (PLA) and poly(D,L-lactic acid -co- glycolic acid) (PLGA).

Methods: The internal osmotic pressure inside eroding PLA microspheres was analyzed with differential scanning calorimetry (DSC) in a temperature range of 10 to--25 degrees C. The osmotic pressure was calculated from the melting peaks of the aqueous phase using purity analysis. For pH determination, PLGA microspheres were loaded with a pH-sensitive spin probe which allowed the determination of pH by electron paramagnetic resonance (EPR).

Results: The osmotic pressure in PLA microspheres increased to 600 mOsm within four days and decreased to 400 mOsm after two weeks. The pH in PLGA microspheres in this study was < or =4.7. Basic drugs such as gentamicin free base or buffering additives led to a pH increase. In no case, however, did the internal pH exceed a value of 6 within 13 hours.

Conclusions: DSC and EPR are useful techniques to characterize the chemical microenvironment inside eroding microspheres. This data in combination with detailed information on peptide and protein stability could allow in the future to predict the stability of such compounds within degradable polymers.

PubMed Disclaimer

References

    1. Biomaterials. 1996 Feb;17(4):457-61 - PubMed
    1. Chem Pharm Bull (Tokyo). 1996 Jan;44(1):235-6 - PubMed
    1. Pharm Res. 1994 Aug;11(8):1143-7 - PubMed
    1. Pharm Res. 1997 Apr;14(4):420-5 - PubMed
    1. Vaccine. 1996 Sep;14(13):1205-13 - PubMed

Publication types

LinkOut - more resources