Skip to main page content
U.S. flag

An official website of the United States government

Dot gov

The .gov means it’s official.
Federal government websites often end in .gov or .mil. Before sharing sensitive information, make sure you’re on a federal government site.

Https

The site is secure.
The https:// ensures that you are connecting to the official website and that any information you provide is encrypted and transmitted securely.

Access keys NCBI Homepage MyNCBI Homepage Main Content Main Navigation
Comparative Study
. 2001 Nov;17(6):512-9.
doi: 10.1016/s0109-5641(01)00011-2.

Dimensional change following setting of root canal sealer materials

Affiliations
Comparative Study

Dimensional change following setting of root canal sealer materials

D Ørstavik et al. Dent Mater. 2001 Nov.

Abstract

Objective: The study was designed to evaluate a method proposed for measuring dimensional changes of endodontic sealers, and to assess the dimensional changes of 11 commercial sealers after prolonged storage in water.

Methods: The method for linear dimensional change described in the draft standard for endodontic sealers was applied to 11 different types of endodontic sealers. One material (Sealapex) could not be tested by the method. The other 10 materials were followed for dimensional change over 48 weeks.

Results: The sealers showed markedly different dimensional properties. For most materials, the greatest dimensional changes took place within the first 4 weeks. Zinc-oxide-eugenol based sealers generally showed shrinkage ranging from 0.3 to 1%, while one product (Proco-Sol) exhibited expansion exceeding 6% after prolonged storage. The epoxy-based materials, AH 26 and AH 26 silverfree, exhibited a large, initial expansion of 4-5%. AH Plus expanded from 0.4% after 4 weeks up to 0.9%. Apexit, a Ca(OH)2-based material, showed only minor variation round baseline value, -0.14 to +0.19%. Roeko-Seal expanded to 0.2% within 4 weeks, but was stable thereafter.

Significance: The test methodology adequately assessed dimensional changes exceeding +/-0.2%, but some brands of material either could not be made into adequate test specimens or showed surface changes which interfered with dimensional change measurements. Theoretical approaches to the consequences of expansion by materials of low bulk strength question the necessity of a strict requirement against expansion, whereas bacterial penetration may be a real threat from sealers shrinking as little as 1%.