Skip to main page content
U.S. flag

An official website of the United States government

Dot gov

The .gov means it’s official.
Federal government websites often end in .gov or .mil. Before sharing sensitive information, make sure you’re on a federal government site.

Https

The site is secure.
The https:// ensures that you are connecting to the official website and that any information you provide is encrypted and transmitted securely.

Access keys NCBI Homepage MyNCBI Homepage Main Content Main Navigation
. 2007 Mar;131(3):301.e9-15.
doi: 10.1016/j.ajodo.2006.01.026.

Three-dimensional measurement of residual adhesive and enamel loss on teeth after debonding of orthodontic brackets: an in-vitro study

Affiliations

Three-dimensional measurement of residual adhesive and enamel loss on teeth after debonding of orthodontic brackets: an in-vitro study

Amna Hassan Al Shamsi et al. Am J Orthod Dentofacial Orthop. 2007 Mar.

Abstract

Introduction: The purpose of this study was to evaluate 3-dimensionally the changes on tooth surfaces after debonding orthodontic brackets and after removing residual adhesive and finishing.

Methods: Sixty premolars were randomly divided into 2 groups, and brackets were bonded according to the manufacturers' instructions. Two types of orthodontic adhesives were used: resin-modified glass ionomer cement (group 1) and resin-coated adhesive precoated brackets (group 2). The brackets were debonded on a testing machine at a cross-head speed of 1 mm per minute. Models were made of each tooth before bonding, after debonding, and after removal of residual adhesive. The models were scanned with a 3-dimensional laser scanning machine, and the scanned images were analyzed by using modified analytical software.

Results: The Mann-Whitney test showed significant differences in adhesive thickness and enamel loss between the 2 groups (P <.001). The mean (+/- SD) thickness for group 1 was 31.2 microm (+/- 26.5 microm), and the mean (+/- SD) thickness for group 2 was 102.7 microm (+/- 79.71 microm). The means (+/- SD) for enamel losses after cleaning and finishing the enamel surfaces were 22.8 microm (+/- 17.67 microm) for group 1 and 50.5 microm (+/- 31.27 microm) for group 2.

Conclusions: Adhesive thickness and enamel loss due to orthodontic procedures can successfully be measured in vitro by using 3-dimensional laser scanning technology.