Skip to main page content
U.S. flag

An official website of the United States government

Dot gov

The .gov means it’s official.
Federal government websites often end in .gov or .mil. Before sharing sensitive information, make sure you’re on a federal government site.

Https

The site is secure.
The https:// ensures that you are connecting to the official website and that any information you provide is encrypted and transmitted securely.

Access keys NCBI Homepage MyNCBI Homepage Main Content Main Navigation
Comparative Study
. 2008 Jun;66(3):159-68.
doi: 10.1080/00016350802123118.

Bonding of one-step and two-step self-etching primer adhesives to dentin with different tubule orientations

Affiliations
Comparative Study

Bonding of one-step and two-step self-etching primer adhesives to dentin with different tubule orientations

Olabisi Asande Adebayo et al. Acta Odontol Scand. 2008 Jun.

Abstract

Objectives: To determine the microshear bond strengths of five 'all-in-one' adhesives and two 2-step self-etching primer adhesives to dentin with different tubule orientations and to compare bond strengths between the adhesives.

Material and methods: Human adult molar teeth were sectioned to obtain dentin pieces with tubule orientations perpendicular or parallel/oblique to the bonded surface. Two 2-step self-etching primer adhesives (Clearfil SE Bond (CSE), Optibond Solo Plus SE Bond (Op. SE)) and five all-in-one adhesives (Clearfil S(3) Bond (S(3)), Optibond All-in-One Bond (Op. AIO), G-Bond, Go!, and Xeno IV) were applied to dentin in accordance with the manufacturers' instructions. Resin composite cylinders were bonded to superficial and deep dentin using microtubes (0.75 mm internal diameter and 1.5 mm high). Bonded specimens were stored in water at 37 degrees C for 24 h, then stressed in shear at a cross-head speed of 1 mm/min until bond failure. Maximum load at failure (N) was recorded and converted to MPa. Statistical analyses were carried out using independent samples t-test and one-way ANOVA with Tukey's HSD test.

Results: Though bond strengths varied slightly, four all-in-one adhesives (Op. AIO, G-Bond, Go!, and Xeno IV) showed no significant differences in microshear bond strengths regardless of dentin depth (superficial or deep) or dentin tubule orientation (perpendicular or parallel/oblique). CSE, Op. SE, and S(3) showed significantly lower bond strengths to deep dentin with a tubule orientation perpendicular to the surface.

Conclusion: Most of the all-in-one adhesive systems used in this study appear to bond equally well to dentin independently of tubule orientation and depth. One two-step self-etching primer adhesive bonded significantly better than the all-in-one adhesives.