Skip to main page content
U.S. flag

An official website of the United States government

Dot gov

The .gov means it’s official.
Federal government websites often end in .gov or .mil. Before sharing sensitive information, make sure you’re on a federal government site.

Https

The site is secure.
The https:// ensures that you are connecting to the official website and that any information you provide is encrypted and transmitted securely.

Access keys NCBI Homepage MyNCBI Homepage Main Content Main Navigation
. 2009 Mar;25(3):283-9.
doi: 10.1016/j.dental.2008.07.007. Epub 2008 Aug 29.

Insufficient cure under the condition of high irradiance and short irradiation time

Affiliations

Insufficient cure under the condition of high irradiance and short irradiation time

Li Feng et al. Dent Mater. 2009 Mar.

Abstract

Objectives: To investigate if and why a plasma arc curing (PAC) light tends to undercure methacrylate-based resins or resin composites.

Methods: Model dimethacrylate resins, commercial dental adhesives, and commercial resin composites were cured using a PAC light and a halogen light with the similar radiant exposures but different combinations of irradiance and irradiation time. The degree of double bond conversion (DC) was measured with FTIR spectroscopy and analyzed as a function of radiant exposure.

Results: The PAC light produced a lower DC than the halogen light for the model resin with the lowest viscosity and for three of the four adhesives. With a high irradiance, the PAC light could cure three of the four composites as thoroughly as its halogen counterpart. When the irradiance was reduced, however, three composites yielded a lower DC.

Conclusions: Insufficient cure by PAC lights or any curing lights with very high irradiance is likely to happen when too short an irradiation time is used. It is because under higher irradiance, the lifetime of free radicals is shorter.